03-25-2014, 10:37 PM
I am selling my double front load annealers. The top annealer has been used less than a handful of cycles and the bottom just to burn out the binders. They are made with 20 gauge stainless steel, except for the tube steel frame. The interior of each annealer is 23" wide X 23" deep X 18" high. Wall construction is 1" frax board on sides, doors and ceiling and a 1" soft brick floor with 2" mineral wool backing for a total of 3" of insulation everywhere. There are levelers on the corners and the doors have cut off switches. It uses standard Duralite elements (2) per annealer that draw only 18.4 amps total for each unit in quarts tubing and the doors have fiberglass tadpole gaskets with t-handle pull latches. They come up to annealing temp in less than a half hour. I am asking $3200 with no controllers. I live in St. Paul MN. Buyer is responsible for shipping.