11-17-2014, 08:17 AM
i want an enameling kiln. any smallish front loader will do. thanks, rosanna

Tom Fuhrman
11-19-2014, 09:23 AM
Rosanna: keep your eyes open for an Amaco enameling kiln, front loader, I've been using one for over 25 years and it was used when I got it. about 14" wide X 6" tall x 18" deep interior dimensions. used they should be about $100-150. I use mine for pickups and a warming oven.

Pete VanderLaan
11-19-2014, 04:47 PM
I have actually seen people do strange and remarkable things with electric counter top toasting ovens that have been reworked with fiber. Don't dismiss it.

Rosanna Gusler
11-20-2014, 03:54 AM
Found one. Thanks.

Eben Horton
11-20-2014, 06:21 AM
I have actually seen people do strange and remarkable things with electric counter top toasting ovens that have been reworked with fiber. Don't dismiss it.

Awe man. That's almost as bad as using a dish washer body as an annealer frame!

Pete VanderLaan
11-20-2014, 12:11 PM
I didn't just use the frame. It still has the original door. All stainless. I made one for my sister too. It hits 1800 easily and I've never pushed it harder than that. All lined with maronite board.

Eben Horton
11-21-2014, 07:57 AM
I know. It's a really cool little unit.