Looking to see if anyone has any Gaffer Blood Orange they are looking to dump.
This was a "mistake" color - under the number LE-066 Blood Orange Lustre.
Would love to get some more if anybody has it lying around, preferably in powder or frit but beggars can't be choosers.

Daniel Sviland - dsviland(at)gmail.com

Scott Novota
10-05-2015, 01:57 AM
Red Luster is going to be your next best color if you are looking for that reduction.

If you are just looking for the actually blood orange color I have yet to find anything like it but I am still on the hunt.

At one time i had over 30 kilos of the stuff. I have used it all.