View Full Version : Little oval stickers
Jeff Mentuck
01-31-2007, 09:27 AM
Hey everybody, I'm chasing down a corporate order that requires some custom little oval stickers. You know the ones that a lot of murano glass has on them and swedish manufacturers as well. Little foil ovals maybe half inch long. any way, I've been doing some searching online and haven't had a lot of luck. Has anyone ever had these things made up? If so can you recommend a supplier?
thanks,
Jeff
Scott Novota
01-31-2007, 09:50 AM
http://www.sticker.com/Wafer_Seals_Foil.html
Scott.
.
Brian Wong Shui
01-31-2007, 12:32 PM
What you need is someone who specializes in Flexographic printing.
I have used AAA Label (404) 355-6128 and Central Label Products (803) 736-1351.
I am sure that you could find someone closer to you.
Pete VanderLaan
01-31-2007, 12:38 PM
Maybe Steve would sell you some UL Labels....
Charles Friedman
01-31-2007, 05:57 PM
Try www.richmarklabel.com They did a nice job for me. 206-322-8884
David Patchen
02-01-2007, 02:48 AM
Those books don't deserve 'parental advisory' labels, they deserve, "Danger--proven to make you closed-minded, ignorant and lusting for emotionally-driven simple answers". I could go on....
BTW, I find it curious the percentage of glass people here who are philosophically 'blue staters'. Seems disproportionately high....or maybe the Bushies are too ashamed and embarrased to speak out....ah, another thread.
Ben Rosenfield
02-01-2007, 08:00 AM
You might also look into a local shop that does hot stamping (aka foil stamping).
Larry Cazes
02-01-2007, 10:05 AM
BTW, I find it curious the percentage of glass people here who are philosophically 'blue staters'. Seems disproportionately high....or maybe the Bushies are too ashamed and embarrased to speak out....ah, another thread. [/B]
Hmmmm....Not really a Bushie but definitely conservative. Guess we just have more important things to do with our time, like learn how to blow pretty glass :) Too much tinfoil hat stuff here and not enough debate about real issues for my taste.
Sorry for the drift.
Kurt Walrath
02-02-2007, 11:15 AM
Mark:
We use Century Marketing 12836 s Dixie Hwy, Bowling Green, OH 43402-9976 800-537-9429 email centurylabel.com
Rollin
Jeff Mentuck
02-02-2007, 05:07 PM
Thanks guys, I think Rickmark has just what I need. :drink: