09-25-2007, 08:06 PM
thanks for the shears Wes!!!!

I spent some time de- rusting them..mig welded the blade back together and then brought the shears up to a high polish.
Also, I heated up the handles and adjusted the blades so they would actually cut glass :D

I will use these for a lifetime... thanks so much. Your tag will be done soon....

http://i111.photobucket.com/albums/n138/surfhoglureco/IMG_0891.jpg

http://i111.photobucket.com/albums/n138/surfhoglureco/IMG_0890.jpg:)

Eben Horton
09-25-2007, 08:31 PM
this was the before shot...

Jeff Hoover
09-25-2007, 09:43 PM
Final results look great!
Please post a pic of the tag before you send it off!

Wes Hunting
09-26-2007, 04:59 AM
Glad you were able to use them, Eben.
Don,t go to all the trouble of making me a tag, thanks for the offer, but I do not need any tools at this point.

Eben Horton
09-26-2007, 03:39 PM
Are you sure Wes?? i just made 3 yesterday and this one has your name on it-

http://i111.photobucket.com/albums/n138/surfhoglureco/glass%20stuff/IMG_0898.jpg

David Patchen
09-26-2007, 06:48 PM
Wes, let me know if you want some tags for real men ;)

http://talk.craftweb.com/attachment.php?s=&postid=64513

Actually Eben, those shears look great--I should send you all my tools for polishing :)

Eben Horton
09-26-2007, 07:25 PM
great a new side business- "the shear doctor"

um David, if you can make a tag as nice as that, you can polish you own friggen tools :p


So does anyone have any broken Dino jacks they dont want anymore???? :rolleyes:

David Patchen
09-27-2007, 03:06 AM
Hehe, touche' :)

Victor Chiarizia
09-27-2007, 06:06 AM
wes, can i have your tag? :<)) Vic

Wes Hunting
09-28-2007, 06:31 AM
Originally posted by Victor Chiarizia
wes, can i have your tag? :<)) Vic

Only if you send me a pizza made in your brick oven. :p

Did you get the bromide I sent?

Victor Chiarizia
09-28-2007, 08:17 AM
no bromide yet. and as for pizza you'll have to do a southern run and come and feast**


**the new brick oven will be done in about a year. vic

Eben Horton
09-28-2007, 10:21 PM
wes i'll send it out to you in a few days...

vic, if i make any more i will make one for you. They are quite easy to make and i actually enjoy making them. Any excuse to use my new nifty mig welder makes me happy. :D


so whos got some bent to shit Dino jacks???? huh???? come on cough em up dammit.. :feathers: