Interesting scalped pot pdf raises some interesting prespectives and aspects concerning electric melting......

http://www.glafo.se/pdf/GT3-98%20_69-73.pdf

Pete VanderLaan
11-10-2007, 02:54 PM
the moly sulphide is not going to be much help and I wonder how difficult it would be to obtain Sodium Antimonate. Just the sound of it is expensive. Straight up Antimony trioxide is bad enough these days. Nitrates aren't all that easy to get without raising eyebrows either.

I have noted over the years that the inclusion of 1 percent Neodymium seems to produce exceptionally clean glass as well. I don't know why. Violet though.

Kraig Richard
11-23-2007, 08:40 PM
Shit that was the wrong PDF.. I'll try to find it again.