Well, I set up my first ramp cycle, etc. Did good. Checked it carefully before and during.
Now, I want to use it again and it won't let me. Stat say it is at End, but when I go to Prog, it won't let me change to Run. And I can't change the set point either.
I suspect the problem is that I did the final set point at 32C (about 90F) which I keep the annealer at to keep it dry and it hasn't gotten down that low, so I wonder if it hasn't "released"
What do I do to break it out now and what should I set to prevent this in the future? I have Mod set to the default, I found the message about using 4 after I came in.

Steve Beckwith
11-12-2007, 04:51 PM
I think that you have to hit the SEL to PROG then select off first.

Brian Gingras
11-12-2007, 05:29 PM
yes set to off first and it will (usually) revert to it's last manual set point. Thats how we use our annealer...when i hit off it ramps up for the day, and then run brings it down.

Tom Bloyd
11-12-2007, 06:33 PM
Push sel and then data and change it to off and then put it into run

Mike Firth
11-13-2007, 01:09 PM
Thanks all, that's great, worked fine. Of course, looking at the directions doesn't suggest that you have to turn program off to finish the process.