02-09-2008, 12:27 PM
- I did not label as I should have when i got a bargain 50pounds of glass a few months ago.... so, I do believe I have photo/light sensitive glass -the more I expose it in the glory hole, the greyer it turns...and the stuff in the annealer was still grey this morn. I don't have a light to make it into glow in the dark, - I do have white and black color that looks nice w/ it....my question is- it is safe to work w/, and expose people to (sell) ????
Donald Feser
02-09-2008, 03:38 PM
---after some research, it is ok. just going to be grey. and nothing in my shop will ever be unlabeled again....she says as she goes to scoop out hot glass....(thank god only added 20 pounds of it..)
Todd Anderson
02-10-2008, 12:21 PM
We had some problems a while back with the air/fuel mixture in one glory hole and was seeing our clear reducing... you might want to check that out...