Im trying to roll my own sheet glass in 96 for use in roll ups. I present it to the rolling machine I made but it either gets stuck on the rollers (to hot I think) or it just cracks before I get any nice sheet. Has anyone tried and made this work ? Im shooting for 1/8th thick. Thanxs, Mike
Pete VanderLaan
03-09-2008, 04:23 PM
What temperature are you preheating the rollers to?
Michael Stevens
03-09-2008, 05:38 PM
My best geuss would be around 700 to 800 F. on the roller preheat.
Pete VanderLaan
03-09-2008, 09:10 PM
you have to get to just below wetting point and I mean just below.