Glasma 104 coe Pelletized Batch, Glasma stock # 3115-33J.
Packed in 25 Kilo Factory bags with batch composition listed.
Approximately 4400 pounds (80 x 25 kilos) available.
Paid $0.65 per pound plus outrageous freight charges from Sweden.
Will sell entire lot for $2500 which is about $0.57 per pound.
Plus freight, unless you are in the Northwest and have a truck.
Makes a very nice soft, clean crystal clear glass.
104 COE calculated expansion.
Can be melted in wire melter at 2250F.
Pelletized, so very little dust on charging.
Call 360.754.9555 if you are interested,
will send samples and/or take offers.
Thanks,
Jed
Packed in 25 Kilo Factory bags with batch composition listed.
Approximately 4400 pounds (80 x 25 kilos) available.
Paid $0.65 per pound plus outrageous freight charges from Sweden.
Will sell entire lot for $2500 which is about $0.57 per pound.
Plus freight, unless you are in the Northwest and have a truck.
Makes a very nice soft, clean crystal clear glass.
104 COE calculated expansion.
Can be melted in wire melter at 2250F.
Pelletized, so very little dust on charging.
Call 360.754.9555 if you are interested,
will send samples and/or take offers.