Mark Dolan
12-31-2011, 06:46 PM
What is the recommended way to turn down a Gloryhole? I'm running a little too hot and need to adjust down. Should I just turn the air down?

Mike Hanson
01-01-2012, 02:03 AM
Turn down both the fuel and air until you reach a neutral flame and the heat you want. Turning down just the air will give you a fuel rich flame.

Pete VanderLaan
01-01-2012, 05:33 AM
And if you don't really know what you're doing there, turn the gas down first.