What is a safe ramp rate up and down the work temp, batch temp, cook temp, squeeze temp and back to working temp? I've been going as fast as the furnace will allow but have wondered if that is to hard on the pot.

Pete VanderLaan
01-13-2012, 09:22 AM
keep it up. You aren't going to hurt the pot.

Lawrence Duckworth
01-13-2012, 11:15 AM
This coming from the guy with taxed patience.....a $500.00 hr. consulting rate and a boat payment.

Thanx,....I think??

Pete VanderLaan
01-13-2012, 12:15 PM