so....say you want to melt 50 kilos of r-41 rod in a gas fired free standing pot,
its a 350ish lb, what temp. would you melt? I will heat the rods to around 1000F
before charging. my first guess is around 1900, think thats too hot?
and no, I do not want to make my own color, it needs to be r-41.
its a 350ish lb, what temp. would you melt? I will heat the rods to around 1000F
before charging. my first guess is around 1900, think thats too hot?
and no, I do not want to make my own color, it needs to be r-41.