View Full Version : canadian refractory question

Lawrence Ruskin
03-31-2012, 10:35 AM
The name of the company near Vancouver BC that got me that kast o lite 30 was Thorpe Canada out in Abbotsford. Cost me $42.90 a bag. 855 4004

Hopefully this will help.

Mark Armstrong
03-31-2012, 04:14 PM