While we are still trying to fine out this stuff (still no luck), I noticed this on a ball I blew a few weeks ago. Hmmmmm

Pringle Teetor 02-26-2020 05:59 AM

This is not a cloudy film on the inside like we had in ornaments with the original spectrum glass. It reminds me of oil slicks on water puddles.

Pete VanderLaan 02-26-2020 07:43 AM

Quote:

Originally Posted by Pringle Teetor (Post 147001)
While we are still trying to fine out this stuff (still no luck), I noticed this on a ball I blew a few weeks ago. Hmmmmm

***
It actually looks like really stressed glass under a polarizer. Sometimes you can see that without a filter.

Shawn Everette 02-26-2020 09:00 AM

I've had that with things that went into the knock off. Need to figure out how to keep it and sell it as "special reserve".