Josh Bernbaum 09-07-2017 03:38 PM

Gaffer G-48 "Durissimo" black
 
Anyone try it out yet?
I thought their duro white was the stiffest thing around. I was wrong.
This stuff made me feel like a beginner at pulling cane again, but man does it hold a fine dense line. Just curious what others' experience yet if any..

Pete VanderLaan 09-07-2017 06:02 PM

Oh shit, you have to see what Mark made. The Italian gov has taken away the toxic enamels from murano . The usage of non toxic opaques is the future.

Josh Bernbaum 09-07-2017 09:37 PM

Look forward to hearing about it Pete