Jesse Bogenrief 03-24-2020 09:10 PM

Shut down
 
I am about to shut my furnace off and rebuild. Looking for opinions i have a thermjet 250 my question is should I pull the head hot or wait till it cools to pull it. Just seeing what experiences people have had. Thank you

Bill Worcester 03-25-2020 01:44 AM

Is it likely stuck in place?
 
If you think it will come out easily when cold, leave it in place. If not pull out hot and wrap ceramic part of the burner in flax to cool slowly.

Pete VanderLaan 03-25-2020 06:50 AM

spell check strikes again; "Flax".

Frax I suspect. It will burn up linen after all.

Art Freas 03-25-2020 08:47 AM

Ours came out easy after we were cold. Though it didn't really matter as ours was trashed and needed to be replaced.

Jordan Kube 03-25-2020 12:07 PM

Don't pull it out hot.

Eben Horton 03-25-2020 07:54 PM

Quote:

Originally Posted by Jordan Kube (Post 147456)
Don't pull it out hot.

Correct. itís only 80% effective in unwanted problems. ;)

Art Freas 03-26-2020 12:28 PM

Don't do anything to put it at risk, those things are expensive. We had to replace ours in our rebuild (it was 12 years old).