Pete VanderLaan 07-01-2011 05:08 PM

Passage Bricks for moly users
 
We are now making Passage bricks for moly disilicide elements for both 6/12 and 9/18 elements. Cost is $35.00 each shipped UPS at cost.

Woo Hoo!