How do you connect these. A 12 g thermocoupler
And a 20g wire. I am thinking about a porcelain twist on connector. What are your thoughts?

Scott Dunahee 11-04-2019 07:03 PM

I always used a ceramic terminal block, Franklin. I think they were thermocouple specific and didn't cost very much. They have them on amazon for $6 us. Hope that helps.


BSD

Eben Horton 11-04-2019 07:35 PM

You could also use a copper split nut

Franklin Sankar 11-04-2019 07:42 PM

Thanks. I can get the block here.
Franklin

Peter Bowles 11-04-2019 10:21 PM

Be sure to get the polarity of the compensating cable the right way round. The cables have specific alloys for the + and - with specific resistance. If you get the cable the wrong way round your temp readings will differ.
There are numerous charts - all colour coded for the different types of cable, and interestingly, none of them yet fit to an international standard so you'll have to match what you have with the appropriate table.

Franklin Sankar 11-05-2019 05:00 AM

Noted with thanks
Franklin

Franklin Sankar 11-06-2019 01:51 PM

I just noticed the block we have are not thermocouple specific. So I am back to Eben coper lug split bolt. I ordered a block also. Just have to sit back and wait.
Never got so much trouble connecting the thermocouple . Itís as if the controller lost some of its sensitivity. It all started when I found the nice doggie sitting on the annealer.
Franklin

Franklin Sankar 11-06-2019 01:59 PM

I pulled the order . Scott or anyone else. What is the name of the block you ordered. Just to make sure .
Franklin

Franklin Sankar 11-06-2019 04:36 PM

1 Attachment(s)
I got this to work . At least for a while.ceramic connectors so no contamination with other metals impacting on the joint.
Franklin

Scott Dunahee 11-06-2019 08:40 PM

High Temperature Ceramic K-type Thermocouple Terminal Block

I just searched amazon for "thermocouple terminal block"

Good luck Franklin!

BSD

Pete VanderLaan 11-07-2019 09:54 AM

I would think that trying to connect a 20 gauge to a 12 gauge wire in a split bolt is fraught with potential issues. The block connector in my mind would be better.