Lawrence Duckworth 09-26-2014 12:20 PM

1 Attachment(s)
I’m okay with the air cooling method, its the delivery system that needs a doooo over....the air cooling system could use a bigger blower and at least a 3/4” radiator type hose and a filter.

Here’s the furnace after 3 winters use (and a little clean up). No problems other than Bussman fuses blowing.

Just finished adding a new pot, air ram to open the door and a ceiling blower to help keep the connections cool.

Lawrence Duckworth 06-14-2015 04:44 PM

a link to some of the furnace build photos I have. (scroll down a bit ) http://lawrenceduckworth.com/untitled.html

Pete VanderLaan 06-14-2015 05:33 PM

Thanks Lawrence, I think that really helps. James Burt has bought the 22.5 KW electric package from me and I'm trying to convey how that front plate works. I've advised him to get the plate and then design around it since he wants to bring the 24 inch pot out the front ( What a concept) . Mine, on the 28 inch electric package tilts back a bit on the back of that casting but presents in essentially the same way as yours. That's a great sequence, thank you.

I really will miss my moly.

I'm about to start a medium size gas unit using an 80 lb pot and two 11 inch pots for the time Scott and I will melt enamels if there is an interest.I could use it as a permanent smaller furnace as opposed to the larger one. It will use a recuperation system Charlie Correll is building. I'll do it from the first weld if there is an interest.

Otherwise I'll just build it.

James Burts 06-15-2015 08:50 AM

Lawrence-

Those pictures are terrific! Thanks for posting them.

As Pete mentioned, I'm going to be taking on a build of a moly furnace, and have been having trouble visualizing some of the casting that Pete has been recommending. Seeing your furnace helps considerably!

--James--

Quote:

Originally Posted by Lawrence Duckworth (Post 124422)
a link to some of the furnace build photos I have. (scroll down a bit ) http://lawrenceduckworth.com/untitled.html


Lawrence Duckworth 10-26-2015 08:19 PM

here's my high tech soft start controller https://www.youtube.com/watch?v=vUyre82myx0 bungee cord

Michael Ahlefeldt-Laurvig 10-31-2015 01:36 PM

That looks real good- great

Lawrence Duckworth 03-03-2018 09:22 PM

Quote:

Originally Posted by Lawrence Duckworth (Post 124422)
a link to some of the furnace build photos I have. (scroll down a bit ) http://lawrenceduckworth.com/untitled.html

This is a link to some of my moly furnace construction photos. Iím deleting this page from my site soon, so if this has any value to anyone feel free to copy it before I remove it.👍

David Russell 03-03-2018 10:28 PM

That some nice work Lawrence my hat is off to you.

Lawrence Duckworth 03-04-2018 12:26 PM

Quote:

Originally Posted by David Russell (Post 138831)
That some nice work Lawrence my hat is off to you.

Thanks to you David and others like you....:) obviously I can follow directions


All times are GMT -5. The time now is 12:54 AM.

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.