Video - Designing and making photochromic glass
Glass engineering - designing and making photochromic glass
https://www.youtube.com/watch?v=mUcUy7SqdS0 Not sure if this video has been posted here before, but it's quite a cool exploration of photochromic glasses, from a non-glass-specialist. This guy has a youtube channel where he makes a lot of interesting videos about projects in the overlap between the physics/chemistry/electromechanical worlds. Was fun to see someone from a totally different background manage to run into such a wide cross-section of the issues that come along with making & melting glass in just a couple months of doing test melts. (If you want to jump right to the batch recipe & discussion of photochromic chemistry, skip to 26:00 or so. The first 25 minutes are mostly focused on equipment, melting process, & ingredients.) |