Franklin Sankar 06-15-2019 02:36 PM

Heater crossing thermocouple
 
My heating coil need to cross over or under the thermocouple.
I am thinking about stretching the coil and slipping it under or over the thermocouple. Any warning or comments?
Franklin

Franklin Sankar 06-15-2019 02:37 PM

1 Attachment(s)
This is a drawing of what I want to do. Hope it donít rotate.
Franklin

Sky Campbell 06-15-2019 06:02 PM

I would drill a new hole for the thermocouple before I would do anything to change the element. Every little thing you do like that causes uneven heating and stress to the element. Maybe just drill and angle the thermocouple above the element.

Pete VanderLaan 06-15-2019 06:02 PM

further away would be better.

Franklin Sankar 06-15-2019 07:44 PM

Thanks . Wise hints well noted

Franklin

Franklin Sankar 06-16-2019 08:15 AM

Sky you mentioned something very important about the groves for the coils but I canít find it now. It was something about the shape of the grove and the reflected heat in the grove.
Can you remember?
Franklin


All times are GMT -5. The time now is 07:47 PM.

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.