Pete VanderLaan 04-23-2019 08:35 AM

I saw some snippets on Glassies regarding the new Czech bobbles yesterday as something people were trying out and liked but I didn't run it down.

There's nothing attractive to me about those flakes at all.

Shawn Everette 04-23-2019 09:51 AM

If you're treating the glass so poorly that you basically have to treat it like batch, what's the point of getting cullet? I've used cutoffs before (not my call), and there is no advantage other than off setting yield loss.

Pete VanderLaan 04-23-2019 10:51 AM

Cullet shortens melt sessions and it's far easier to top a pot off with cullet and to not have to consider volition loss. Then you can start in on the downsides of cullet but from my chair, I don't see people actually caring about glass quality at all. That's disheartening.

I want my glass right, seed free, high luster taking color really well. I'm in a minority it seems. This cullet war will not serve people well. Who has the capacity to deal with a 2000lb supersack? Who wants candy bar cullet that will explode in the pot? Who wants dirty Grade B cullet from Cristallica? Parriot will probably have a good product. He's a smart guy but I doubt the ability to meet demand. 11 tons a week is a lot of glass and I think that's about what the US demand is.

And this doesn't address mismatch at all.

Shawn Everette 04-23-2019 11:36 AM

True, it does flatten faster, but all of the cutoffs need to be taken to full charge temp to fine out. The at gather temp charge was what I saw as the main advantage of the A grade nuggets and bird droppings. It was slow, but tanks stayed fresher longer, and I wasn't beating the hell out of my furnace.

I'm in line for the Parriot, and can buy volume, so I hope to stay ahead of the supply curve. As long as it's cleaner with the off gassing than the original cristallica I should be happy.

Pete VanderLaan 04-23-2019 12:08 PM

waht will it cost. I assume about .12lb to ship it. What kind of volume and when?

Shawn Everette 04-23-2019 12:58 PM

We're looking at $1.40, shipping was $.115 last time I got anything. Still looking at at least a month out for the bags, cristallica 3+.

Pete VanderLaan 04-23-2019 01:37 PM

Nobody is making any money at all at that price. I view that as bad.

Franklin Sankar 04-25-2019 05:09 AM

What do you mean by........all of the cutoffs need to be taken to full charge temp to fine out. ???
Franklin

Pete VanderLaan 04-25-2019 06:57 AM

the bubbles don't come out easily unless you go to batch temps.

Shawn Everette 04-25-2019 09:50 AM

The problem with the cutoffs is that the way they are produced and packaged leaves them covered with a lot of fine particulate and dust, hence the need for batch temperature. Most of the old nuggets from Spectrum and bird droppings from Cristalica were clean enough to not have to change temperature, if you were patent enough. It was generally a good rule to save the last little bit from each bag for the last charge, they were fairly dust free but not perfect. What both companies are delivering now is less than desirable from that perspective.

Franklin Sankar 04-27-2019 11:19 AM

Oh so the cut offs are the cullet and they are dirty.
Thanks
Franklin

Pete VanderLaan 04-27-2019 01:43 PM

dirt and dust are major problems on cullet. You can spend days trying to get glass dust to go into solution without gas.

Shawn Everette 04-27-2019 02:28 PM

The cutoffs are "cullet" in the traditional sense, that it is preformed glass that is being essentially recycled; much like the old days of using factory marbles or phillips glass. In those cases you would take it to full charge temp, either by itself or mixed in with batch. It's not the more modern vernacular that would be a partially made virgin glass that was designed to go into its first full melt.

One of the main problems with the original cutoffs and I believe the first version of Studio Nuggets and possible this new stuff, was that it was formulated to be fusing glass first, and then just advertised to glassblowers. This is what was causing much of the off gassing and corrosion troubles that was dealt with in the "new formula" and "premium" nuggets.

Cristalica has some of the same issues despite being designed as a blowing glass, but was shipped much cleaner so you could charge lower. Spruce cullet had major production flaws that led to it's early abandonment. Off the line Bomma looks gorgeous, but we'll see if it can keep pace.

Pete VanderLaan 04-27-2019 03:54 PM

My impression with the Spectrum cullets is a bit different. I feel strongly that it never really completed the melt cycle before being pulled from the tank. It appeared mostly melted but was still in an outgassing mode. The boron in that instance was quite active and went after any fireclays or alumina parts.

Boron by itself is not a monster but if you couple it up with barium it can really cause issues. American refractories of typical composition from 76-90 percent alumina are pretty receptive to degradation. The 76 composition is typical of a mullite mix and the 90% is typical of several crucible manufacturers.

But because it processed out of the furnace prior to true fining, it indeed saved money but the chemical reaction resumed once the stuff was melted a second time. The Flake, which Oceanside is currently offering up is stuff I suspect to have boron present. Cristalica has the issue of containing both Boron and barium. They said they had lowered the boron content but all along their literature indicated the amount to be constant. The real problem there, as I see it is trying to ram 7 tons a day through a system designed to process five. Grade B indeed. Whether any of these companies can meet volume demand will be the big issue.

Shawn Everette 04-27-2019 05:00 PM

I actually agree about the Spectrum melt, I'd say about 90% cooked before it was shipped. You could tell easily by comparing the nuggets to the bird droppings, tonnes of bubbles against something relatively water clear. There was also a handling issue with the nuggets. Not sure what kind of juggernaut packaging system they were using, but they usually came out of the bag in rough shape. Although that looked like it was cared for like a new born against the "flake" or the cutoffs.

Chem wise I'm not as nuanced, but there was a major difference switching from 2.0 to cristalica. I had a girder above my flue that collected but a dusting of Boron over 3 years from the Premium. There was 3x6" cake built up after 6 months of cristalica. I was actually surprised by how uniform that stalactite formed, didn't get a chance to preserve it before it fell.

System's and spruce's original follies seemed to be quality over quantity then flipping the script. Cristalica seems to be following suit. I'd wish one of the window plate companies would get in the game, the quality and quantity a single factory is able to process in a day would meet US demand for a year. Maybe not quite that fast, but those behemoths are a sight to behold.

Pete VanderLaan 04-27-2019 06:28 PM

I'll freely admit to being the one who brought Cristalica into the US. I invested in it. After getting the early test materials here, I was discouraged by the melt results. I told Andreea, who won't comment any more here about the boron issue. I offered to do a re-write and was turned down which did not surprise me. They had their money in Peter Kuchinke who then had this remarkable come to Jesus moment a few months back. He bailed in a humiliating public way. I had pulled my investment out of Cristailica about a year earlier and things turned to shit really fast.

Now, I suspect that the increase in output pushed in Dobern had an effect on the output snips and they weren't pretty. The dirt? I don't know but I do know that furnaces of the type are ingenues. Treat them right or they shit the bed.

Pete VanderLaan 04-27-2019 06:31 PM

I'd wish one of the window plate companies would get in the game
[/quote]

**************

Not at $1.41 per lb.

Shawn Everette 04-27-2019 10:08 PM

For what we expect for quality 1.40 is a fortune

Pete VanderLaan 04-28-2019 07:42 AM

No, for what you "Accept" for quality.

Shawn Everette 04-28-2019 08:41 AM

True, society has lowered my standards of acceptance. Sometimes you take what you can get.

Pete VanderLaan 04-28-2019 09:28 AM

It's a forced acceptance unless one wants to either make their own glass or to use another commercial batch glass which requires concerted effort on the part of the facility. Having been down this shortage crisis road more than a few times and having limited volume needs, I get to use my own stuff. Often, it is admittedly a nuisance bu given the freedom of coloring it, I'll go this way everytime.
But until one cullet shows up that delivers a reasonable quality as well as supply capacity, this will continue to be a crapshoot with work stoppages. Parriot's stuff seems to bear promise right now but then again, few have tried it and supply hasn't really been stress tested. . We thought Cristalica would fill that role and it has failed as has Kugler apparently in terms of acceptance. Even so, if anyone wanted to actually make a decent clear glass in the USA, it would be a no brainer. Fundamentally importing clear cullet from Europe is nuts.

You would think someone would objectively field test this stuff and adapt based on the feedback. Right now? Eat your vegetables.

Shawn Everette 04-29-2019 09:18 AM

Yeah, no options state side anymore seems quite odd. Importing from Mexico is bad enough, but shipping it across an ocean is indeed kind of insane. Spruce mixes great glass, but I didn't have confidence that they would have the infrastructure to maintain a cullet operation. System seemed to be starting to function properly before it went tits up. The formula changes gave the appearance of adaptation, but the roll out could have been managed better. While the dust would vary batch to batch, I never really had any problems with any of it.

Turbulent grad school experiences forced me to be flexible with the glass I'm using. I'm happy as long as it's relatively cord free and fits the standard colors. I pull cane as I need it, so I'm not beholden to what's a few decades old. "Intelligence is the ability to adapt to change".

Art Freas 05-03-2019 11:41 AM

On the Oceanside

My matrix on it would be

If the oceanside is like
Original System 96 Studio - OK but to short and too much borax and all the yellow crap.

New System 96 Studio - Would be fine with this longer that the original system 96 but not too long for production.

Premium nuggets - No way the original premium had lots of problems.

Premium 2.0 - Could live with it, nice and long for one offs a bit long for production.

Shawn Everette 05-03-2019 03:11 PM

That's about my take on it too. Judging only by the off gassing alone the new Oceanside is either just their sheet formula or the original Studio, and I'd prefer not to cook any of it.

I didn't really run into issues with either Premium nor the New Formula Studio, but judging by how long it took to get the Flake, I'm not planning on waiting it out for something better.

D&L is the only US distributor for the flake right now. While I've had great experiences with them, they're primarily a wholesaler with steep demands. That will be problematic for any small scale buyers.

tomak baksik 05-06-2019 04:49 PM

glasma
 
1 Attachment(s)
Hi, I have have older pic of glasma bag, this may help:


All times are GMT -5. The time now is 07:27 AM.

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.