I'm having trouble finding information on how people are vacuum encasing these days. In the past Schott S8 pucks were the glass of choice - Are people just running through stockpiles of existing stock? Are small runs still being made for private group buys?

Can this technique be performed without S8? Is it possible to produce something similar from batch or will the clarity/flow always be materially inferior?

Ted Trower 10-16-2019 11:50 AM

best option
 
https://preciosa-ornela.com/en/produ...a-optical-rods

These are 96 glass and have excellent optics. It's what Clinton Smith and Richard Loesel are using. If you are serious email me and I'll give you the correct person to contact there. Shes seems to be the only one who deals with low volume / direct sales. Much of this stuff is used for making automotive headlamps.