Hey, Look! We use a lot of "hothands" back here in our gloves and boots. The big ones last 18 hours. I finally decided to test a simple chemical oxygen theory and as fast as I use some big ones and came inside, I put them in tight aluminum foil and they went cold instantly. Later in the day, I used them again and unwrapped them and they got hot again in a few minutes/ I did the horse maintenance number and re wrapped them for tomorrow.

Call me cheap but they are about .70 for the 18 hours and I use up to eight of them in each boot or glove. It adds up if you have to overpay for Venice.