I would recommend the 19 inch pot from High Temp in Portland. It's a better pot for less money and you don't have to wait for it.

Don't ask them about horseshoes either. They know nothing about them.
Put the ten inches of frax on the crown and eight around the outside. More is simply unnecessary. I would suggest recuperating it. Wake up Hugh! If you do recuperate, the burner needs special consideration and Hugh does sell them I think. I've seen them work and they do it well.
Phlocat will work fine as a crown. Morco 95 would be better but it's hard to get.