oh brother...I read the specs too fast:

English and Turner calculated C.O.E: 87.3 F < Measured C.O.E: 96-97 x 10^7/deg. C

Thanks David, for the clarification.

So...bullseye does NOT offer a product you can use with furnace glass. As you said, Sys96 is the only way to go for the sheetie stuff.