There is always a temptation that "more is better" in opals. It's not the case. Less is better is really the approach. Just right is better still. Calcedonias in my experience want very little silver, and if the tin gets too high, it will reduce everything in sight and turn dark. It has a lifetime in the pot as well. Atmosphere also matters- nice and neutral.
I don't believe I've ever drilled a pot with metals, at least not since about 1974.