Thanks for the help guys, I'll give those things a try. I'm using a CC pot and it's holding up pretty well. Those 38 pound pots are just the perfect small pot.

Dave, yes, trying for more density, one strike wonder. When I make it into bar and pick it back up it is perfectly wonderful and homogeneous. The stuff out of the pot is gorgeous too, just a different animal. What if I melted a pot, scooped it out and then remelted it? Would the glass in the pot strike out like the bar? If no one has done this there is only one way to find out!!!