Alright, looks like I've got some work to do. I'm getting closer to a nice copper blue with silver. The third melt is happening today. The erbium glass is now almost dead on in expansion and hopefully will go into production. Second test for that next Tuesday. I'd really like to loosen it up a bit, it's pretty viscous stuff. I'm wondering if our good friend strontium could help?