My offhand thought is cryolite= sodium alumina hexafluoride/ Very small additives would reduce the melt conditions. It would slop it up. Otherwise sodium nitrate for the runny goblet people. . Either will push the expansion around.
What you need to be seeing is the phase separation reduction of Apatite crystals occurring because the calcium is being dropped. Trying to do this in essentially a production shop is really ambitious.

This is a phrase that really gets spell check maxed out. Now it wants appetite.