Thank you Josh and Pete! I appreciate your input. We have been discussing melting half a bag of batch (10kgs) to test and see through a bit of trial and error. We have an 80kg colour pot furnace and want to melt some tests in the same atmosphere.

Interesting you ask about Gaffer batch re potassium or sodium. I can probably look up the MSDS. I like the idea of Manganese. Also just upping the Pot. Dichromate. We will just be blowing it straight and not trying to fit it with any other glass or colours so at least that is something we don't need to worry about.

Thank you for the note about the coffee grinder! And I look forward to any further information you can add, many thanks Pete