Keep it fresh. I put it in totally sealed cat food containers on arrival. I do that with potters plaster and high alumina castables as well. If the plaster still works after two years in a new Hampshire summer, , I know the containers are doing their job. We must have a few hundred of those Delicat opal white containers with lids. I am amazed at how many of them that cats one and two went through. It was a sad moment when they quit using those things. You can buy the empty containers new on Amazon but it's ridiculously expensive.

I could lash ours together and make a raft like they did in Kon Tiki.
__________________
Where are we going and why am I in this basket?