Gaffer upped the standard for bubble less rod and even concentricity, but certain runs still had issues. I've seen some really funky bars from reichenbach and kugler, but they've gotten better over the years. I don't use rod a ton, and when I do I'm usually marbling it like taffy, so whatever bubbles are there will pale in comparison to what I introduce.

Some people are still diehards for rod, but to me the best advantage frit has is simply speed, for those with out a color pot. Then there is also the color puke aspect of frit mixes, which always seems to be the first ones to sell.