Hi Pete and Peter,

sorry for the delay in responding! Thank you so much for your replies and additional information. I would definitely heed your advice regarding the dichromate vs Iron Chromate. It is wonderful to get your opinions on this.
We do have a wedge mould for colour tests that we use. Initially we will melt small test batches, possibly 10 or 20kg melts to make sure we have the mix right, then we would melt an 80kg pot furnace. Our 400kg tank furnace is only used for clear.