I have been using S96 regular nuggets for about three years, in a 200# moly melter, I am just starting on my fourth ton. I have no door vent, however I do small charges over a 24hr period, and vent the chamber by opening the door between charges for a few moments, I have no evidence of corrosion, any where. I have a slight build up of yellow fluff on the top of the door arch which i remove, at my last cleanout my pot looked very good, I never fire my furnace over 2000 F. my glass is clean and bright. it may take an extra day to fine out. but low and slow is the way to go.