I found a bucket with 50lbs of spectrum white glass in the studio. It looks like busted up sheet. I think I bought it in 2011 for a resident artist's project that never came to fruition. Does anyone know if it's 96 coe or what it is?
I'm attaching a photo. I'm wondering if it would be good for casting into Plaster silica, any insight appreciated.
LT
If it's Spectrum it's 96. Does the bucket have any labels?

You can cast with it. You'll probably have some minor surface devit issues, but nothing outside the norm.