fenton red bubbles

We melt fenton red cullet on occasion. It is a cad/sel red. It was a casting glass for them. When I melt it I have always had to squeeze it and leave it around 2040 F or else we end up with lots of large bubbles( reboil is what I've heard this is called.) I would like to hold it at a higher temp than that. As well as I would like to know whats going on with the bubbles and where are they coming from. It doesn't seem like they will just rise out and go away. Thanks