Thread: Phosphate Opal
View Single Post
  #3  
Old 12-03-2006, 03:18 PM
Rich Federici's Avatar
Rich Federici Rich Federici is offline
Registered User
 
Join Date: Feb 2003
Location: Vineland, New Jersey
Posts: 175
Rich Federici is on a distinguished road
Thank You Pete,

I will see what it looks like tomorrow, Maybe sitting all day helped to fix it some.

The neat thing that I see with the small pieces that pop off the punty is that when you hold them up to the light, you can see that reddish orange glow near the the thinner edge. It looks like they are lit up from the inside.
__________________
Rich
Reply With Quote