Fuji PXR3 controller?

Was wondering if anyone had a trick to resetting this controller. I had a power outage and restarted my hot furnace. Seemed to run through the ramp sections OK until it got to the 5th ramp which I had set to hold the working temp 2170. So as soon as it hits this temp it goes directly to the shut down program 6th ramp. I did not change anything so something must have been reset. tried to find a setting that would allow unlimited time once working temp is achieved, but all the manuals have you set a ramp time with a max 99hrs 59min. Any ideas would be appreciated. Thanks Paul

labrieglass.com