Worked with the 96 for many years, never a fit issue. Had the furnace eating issue, but that was when we were electric, since switching to gas fired, no problems. Tried the premium, had many fit issues, all in our cut/polished solid work, Olympic said they tested the colors against SP and the Premium (done at spectrum though) and all fit/matched, which of course was BS and pissed me off. Back to the 96, which has been very consistent over the years and bullet proof for our solid work with both Reichenbach and Gaffer...