Originally Posted by Pete VanderLaan View Post
I recommend 8 inches as well and I documented the diminishing returns on insulating about ten years ago. I set a furnace at a floating temp with fixed settings. I kept adding insulation and the temps kept going up with the fuel input constant. After eight inches, it stopped changing. It didn't drop after 12 inches, it just didn't change at all.

Enough?
And.. if you stuck a thermocouple in the insulation at 8 inches, you would see that the tempature of the insulation would in increase dramaticly as you added more and more. So, when you are idling at 2000 and turn the furnace up to charge, you would have to heat up all of that hot insulation..