Is anyone using Gaffer's new "Durissimo" black? It's crazy stuff. I've found that with my setup, if I don't preheat to 1250F it cracks after going to hole. It has to be the only thing in my pickup oven at the time of course.. For comparison, the other Gaffer opaques I take to between 1075 and 1130 depending on color.