My two go-to brands for annealer controllers are Aubers or SOLOs.

They both strike a good balance between value (prices range from $50-$150) and reliability. I have used them on several kilns & ovens and have never run into issues, although I'd probably go a little more upmarket if I was buying a controller for a furnace.

Aubers are a little funnier to use, you set temperatures digit-by-digit instead of changing things a degree at a time like most controllers. Not too bad once you get used to it though. SOLOs handle similarly to most other controllers.