uv delamination

Hey ya'll. So I'm trying to help out my partner on a restoration project at a museum. She's got an assembled cut and polished piece that is starting to get the tell tale delam ferns growing at the seams. There's an odd oil slick look to part of it, which I haven't come across before. We think that it was bonded with a UV, which I know is not our favorite. Anybody have experience on how long to expect complete failure?