This is what the artist should do. If he won't, this is what I would do. I've taken pieces off of bases by bringing them up and down through another annealing cycle. The UV turns dark brown and fails. It isn't easy to get off but a super clean razor blade and some acetone should do the trick. Maybe a cork belt and cerium if it's really stubborn. Then re-assemble with hxtal.