On their website Cristalica lists the advantages of using their glass, one of which is:

"CRUCIBLE/FURNACE LIFE: Cristalica glass does not consume your crucible. At least 4 times prolonged crucible lifetime is detected at users of pre-molten material."

I was in contact with Cristalica a few months earlier and they actually recommend Magma's crucibles. But then again there's not much choice.