Hi Jordan, I'm paraphrasing your last entry on the 5% Brossphate post:

"Added half of Dave's borax after reading boron was helpful, added .75% cryolite for same, ... Just need to adjust expansion now."

Was the "adjust for expansion" not needed?

I'm really only interested in doing this at lower temps...2200 max. It melted fine with the full amount of borax so I'll work with that. It did seem to have a sweet spot in the pot so I'll have to work on stirring more.