My issue with SP on custom mixing has remained the same: Cleaning the mixer. At one point when I was doing color work for Josh Simpson's corona platters, he wanted SP to mix it and I said I doubted it would work. I had done the mixing at that time. It didn't work. There were some ruffled feathers and when questioned about cleaning the mixer, Tom said "You have to ask to have the mixer cleaned."
I'll leave that without comment.

The smaller your mix, the greater likelihood for error. Maybe Dave would mix and sell it to you.

SP color base isn't really mixed at all as I understand it. The proportioned chemicals are put in bags. You have to do the mixing.