I have no doubt that the way the nuggets are treated is remarkably different, or that the formula is tweaked from the base clear, I've melted the flat scraps. Just doesn't explain why system "96" sheet glass would be compatible with system "96" base cullet, with it's measured coe of 94, and not also be 94. If the sheet is a true 96, then why is it compatible with a 94, but not all the other 96 out there?
The sheet glass was measured to be 94 not 96. The original studio nuggets was compatible with that sheet glass. The last spruce pine clone made by spectrum was 96 some colors work some will not. That is in my experience and testing from a trusted source.